Does anyone have or know where I can find CTE values in high temperature ranges? Particularly RT to 2200°F for 300 series stainless, 400 series stainless, tool steels, and high-speed (M series) steels. Matweb and other online sources only seem to go to 500°C (~930°F) for the steels I'm interested in.
 
Replies continue below

Recommended for you

Here is reference that has some extrapolated values on different SS. The last pages have some specific range of values for different alloys.
It is hard to find a usable number for CTE since the materials only see these temperature in transit and the number are really meaningless.