Hi everyone,

I have cold bend tubes of SA 213 GR T11 (PARENT METAL NO. 4). Tube size: 50.8mm OD x 4.5mm thik., And bending radius 100.


So, as per IBR code which heat treament cycle shall be follow for stress relieving.
 
Replies continue below

Recommended for you

What does the IBR Code require? Do you have a copy??
 