We are presently taking 5/8 dia. wire and forming it into a parallelogram shape. The die section is split into two pieces and has a six thousandths press fit into a casing that is 5.810 dia. and made from 4340 unheattreated material. We experience some loosening of the die after running approximately one hundred thousand parts with it getting progressivly worse until a new casing has to be used. I was wondering if the 4340 material is the best choice for this and if I might not be better off using the shrink fit method instead of press fitting. The die section must be split due to some finishing, etc. that are easier to accomplish with it being split.