Hello All,

I was wondering if there is anyone out there that can help me understand the two processes. Is there a difference between the two? which is more reliable?

Thank you,
FGY
 
Replies continue below

Recommended for you

Sheet product?
These terms would be used interchangeably.
The question is was it HT after the final cold work or is it left in the cold worked condition?
If left cold worked it would usually be called 'as cold reduced'.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 