Hi all,

My first post here - go easy on me.

I am trying to familiarize myself with ASME IX by working through the code and its interpretations.

One that is throwing me off is QW-200.4(b)- Interpretation: IX-10-34

Subject: QW-200.4(b)
Background: PQR A is welded with SMAW to join 5/8 in. (16 mm) thick plates with 5/8 in. (16 mm) of SMAW deposit. PQR B is welded with GTAW and SMAW to join 5/16 in. (8 mm) thick plates with 1/8 in. (3 mm) of GTAW and 3/16 in. (5 mm) of SMAW deposit. PQR C is welded with GTAW to join 3/16 in. (5 mm) thick plates with 3/16 in. (5 mm) of GTAW deposit.

Question (1): Do PQRs A and B qualify the combination WPS for a base metal thickness range of 1/16 in. (1.5 mm) to 11⁄4 in. (32 mm) when impact testing is not required?


Reply (1): No.


Can someone tell me why that wouldn't qualify that thickness range and what the actual thickness range would be?

Note that part 7 of that interpretation also says this:

Question (7): Do the provisions in QW-200.4(b) affect the responses to the above questions?
Reply (7): No.
 
Replies continue below

Recommended for you

When combining PQRs, the lower of the qualified thicknesses becomes the limit for the WPS.

Based on PQR B, the GTAW process is limited to 5/8" max. base metal thickness (2T), and 1/4" deposit thickness (2t). PQR A is welded on thicker material but does not use the GTAW process, so it doesn't help for T > 5/8".

The question in the interpretation is a bit daft in describing PQR C, which is not referenced in the ultimate question.
 
Thanks brimstoner - where in the code will I find evidence to support that (i.e. the thinner of the two coupons is the range qualified)?

Regarding PQR C, there are other parts to interpretation IX-10-34 (questions 2-6) that reference it.

Cheers
 
ST95,
It is dealt with in 200.4 (a)
(2) the base metal and deposited weld metal thickness
limits of QW-451 for each process, filler metal, or set of
variables are applied.
The base metal thickness limits using GTAW (PQR B)are 2 x T = 5/8"