Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations IDS on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Compaction Trail - to finalize number of rollign passes required to achieve required compaction

Status
Not open for further replies.

mah1r

Civil/Environmental
Feb 25, 2016
1
Does any one have a format to determine number of oasses required to achieve compaction "( for road works - ( subbase / asphalt )
 
Replies continue below

Recommended for you

unless you have prior experience, do a test fill and get your QA/QC crew to observe and test for density. once you do that you can specify the rolling pattern and method
 
Test strips are commonly used for asphalt placement to determine rolling requirements; however, the process can be used for base materials as well, though you can expect more variability with the base material than with asphalt.

Do a search on the following string and you'll find lots of references to test strips....

"FDOT Test Strip"
 
Additionally, thickness of the lifts and types of equipment can affect compaction.
 
Agreed on the comments. As far as asphalt, which has changed considerably over the years, my observation historically has been as follows using a nuc gauge on backscatter. Mat laydown by the machine with a vibrating screed was what I'd ballpark at essentially 88%. Each vibratory roller pass picked up 1 to 2% density. Our State spec is 93% minimum compaction. Watching the growth curve generated during the test strip, one can get a feel for the number passes. If you don't see density between a minimum of 2 to 4 vibratory passes (I count "1 up = 1 pass", "1 down = 2 passes", ...), something is wrong This is where science gives way to art. You have to watch for overlapping passes, tearing at seams, shoving, travel speed, ... Way more to a good product than just passing density.

Earthwork is even more subjective, but watch for the sheep's foot pads starting to walk above the lift. You now also have moisture as an issue and I you'll be looking at the overall depth of the fill, lift thicknesses, ... gravel will be a little more straight forward. Most of the time in my area, proof rolling with loaded tandem is using to proof roll the subgrade and base before proceeding to paving.
 