canwesteng
Structural
- May 12, 2014
- 1,709
Suppose you have a composite member (built up T, but it could a W section or any similar built up section), what is the consequence of welding on only one side of the web to resist shear flow between the flange and the web? I'm thinking either a) nothing happens b) there is flexure in the weld and it breaks c) there is some weak axis bending in the section.