serrojo
Civil/Environmental
- Jan 18, 2010
- 50
Hi to All!
I have found a difficulty finding an example of joint between a regular plain slab and a composite slab.
The problem is that I need to create this joint in an unusual place (middle of the span), we are trying to figure out the solution to cast in-situ slab over prefabricated bathroom pods. Unfortunately we don't have to much space between the top of the pod and the bottom of the slab (say about 35cm).
So I am thinking of using a permanent formwork, and just leave it there. Maybe a steel deck would do the job, but I need to figure out how to support one end of the deck.
Any ideas/ suggestions/ warnings would be much appreciated.
Thanks in advance,
MSc. Eng. Serguei Joa
Structural Engineer
Bouygues Batiment International, Cuba.
I have found a difficulty finding an example of joint between a regular plain slab and a composite slab.
The problem is that I need to create this joint in an unusual place (middle of the span), we are trying to figure out the solution to cast in-situ slab over prefabricated bathroom pods. Unfortunately we don't have to much space between the top of the pod and the bottom of the slab (say about 35cm).
So I am thinking of using a permanent formwork, and just leave it there. Maybe a steel deck would do the job, but I need to figure out how to support one end of the deck.
Any ideas/ suggestions/ warnings would be much appreciated.
Thanks in advance,
MSc. Eng. Serguei Joa
Structural Engineer
Bouygues Batiment International, Cuba.