muffinator_777
Mechanical
- Sep 18, 2023
- 17
Hi,
I have been trying to make a reasonably large composite piece and each time I have attempted it. The composite has gotten stuck to the mold. For reference, the first time I made it, I used spray adhesive and that was the main issue. This time, I didn't use it but the part still seems to be very well adhered to the mold.
I was wondering if anyone has any idea why this might be occurring or would be able to offer any assistance with regards to its removal.
Thanks
I have been trying to make a reasonably large composite piece and each time I have attempted it. The composite has gotten stuck to the mold. For reference, the first time I made it, I used spray adhesive and that was the main issue. This time, I didn't use it but the part still seems to be very well adhered to the mold.
I was wondering if anyone has any idea why this might be occurring or would be able to offer any assistance with regards to its removal.
Thanks