Engr83
Structural
- Dec 6, 2012
- 5
When you plot the three different water-cementitious material ratio, will the sand content change as well?
All three mixes they are plotting have the same #57 stone but
Mix 1 has low cement low water high sand
Mix 2 is middle of the road
Mix 3 has high cement high water and low sand
Should all three mixes contain the same amount of sand and #57 and only the cement and water change?
Thanks.
All three mixes they are plotting have the same #57 stone but
Mix 1 has low cement low water high sand
Mix 2 is middle of the road
Mix 3 has high cement high water and low sand
Should all three mixes contain the same amount of sand and #57 and only the cement and water change?
Thanks.