SperlingPE
Structural
I am looking for an equation to predict the amount of drying shrinkage in a concrete footing.
The footing sides will be formed by grade.
Depth of footing will be 30"-36". Width will be 8'.
Reinforcing will bar mats at the top and bottom.
The footing will be excavated in an existing building.
We are trying to predict how much concrete shrinkage to expect.
Specifically, what will the elevation of the top of the footing be after curing/drying.
The footing sides will be formed by grade.
Depth of footing will be 30"-36". Width will be 8'.
Reinforcing will bar mats at the top and bottom.
The footing will be excavated in an existing building.
We are trying to predict how much concrete shrinkage to expect.
Specifically, what will the elevation of the top of the footing be after curing/drying.