I am trying to repair a concrete sidewalk which is approximantly 400' long. Currently various sections of the sidewalk are breaking apart and becoming uneven. My orginal plan was to remove exiting sidewalk and soil beneath. Then refill excavated area with compacted sand (95% dry density) and repour a new sidewalk. New Sidewalk would be 4" thick with #4 rebar at 12" O.C. in both directions. New sidewalk would have control joints every 5'.
It has down been proposed that we should instead pour a new 4" thick sidewalk with rebar on top of the existing. I am concerned that this will result in future probelms. Any comments or suggestions.
It has down been proposed that we should instead pour a new 4" thick sidewalk with rebar on top of the existing. I am concerned that this will result in future probelms. Any comments or suggestions.