This is my first posting in this forum . I am a Metallurgist and I have a RFQ for a concrete sinker block with bellmouth and lifting attachments.

A concrete block is to be cast with weight measuring upto 20700kgs ( pl see a image of the arrangement).

My concern is about the concrete density 3tons/cu.m . Literature states that density of mortar is 2.400tons/cu.m

Is there anyway we can achieve this requirement of 3tons/cu.m?

The only other requirement is load test 1.5X the calculated weight.

Thanks in anticipation.
25B9254B-D29A-4346-9065-7574423761DC_1_201_a_il2rsx.jpg
 
Replies continue below

Recommended for you

arunmrao - "Heavyweight" aggregate, such as steel or iron, can be substituted for stone aggregate used in typical concrete mixes. The 3 tons / m3 density you need is reasonable. Heavy concrete is used for radiation shielding and certain other special applications. Here is a brief description:
Heavyweight Aggregate

[idea]
 
Thanks SlideRule Era for the link. I was considering using steel scrap to increase the density. However, I was concerned if this would be considered as a composite mixture and land me into problems.

In the past we have cast heavy cast iron weights for offshore structures, lifting cranes etc. But I have no experience in making mortar blocks.

Thanks once again. I shall come back requesting for tips to cast sinker block without any cracks and achieving the weight.

 
2.4 to 2.5 tonnes per cubic metre is normal weight concrete. Can you just make the block larger?
 
Thanks, hokie. The customer insists on 3t/m3. I have offered my quote accepting the technical conditions. I shall come back for more assistance if my bid is accepted.

 