OSUCivlEng

Civil/Environmental
Jan 12, 2009
275
I am working on the design of some concrete slab track. I have a more senior engineer who is helping me, and he has some methods of his own that he has developed.

I have been looking for more information about designing slab track, but haven't had much luck. AREMA has some discussion in the commentary about referring to a PCA document and an ASCE journal from 1951 for the design.

Are there any design methods or a good document to refer to?
 
Replies continue below

Recommended for you

What is the use of the track? What type of traffic will it have? What are the loads and their frequency?

We need a bit more information in order to help.


A Great Place For Engineers to Help Engineers

Follow me there.....
 
It's for a railroad siding at a flour mill. Per AREMA it has to be designed for the standard Cooper E80 loading. The rail will be attached to the concrete slab with direct fixation fasteners.

I found a good Advanced Strength of Materials book by Hartog that discusses beams on elastic foundations. I can use that to calculate a bending moment in the slab and size the reinforcing. I will refer to CRCP design methodology for the transverse reinforcing to control cracking.

PCA recommends beams on elastic foundations or finite element analysis.
 