I have a concrete pump station project under construction. The material lab has flagged a specific test for failing the field slump test. At the same time, the cylinder passed the 28-day break test.
The mix specification is one of the State highway department's mixes, so it is well documented and very common. There are no fancy additives to my knowledge.
Should I be concerned? The slump was 7.75" and the max allowed was 5.5".
Thank you in advance.
-Joel