Hi,
We have observed spalling of concrete upon de-shuttering the soffit formwork after 25 days. The concrete slab is 2.0 meter thickness and was poured using 45 Mpa mix with 35% flyash to meet heat of hydration requirements as the thickness is 2.0 meters.
Test cylinder samples have achieved the required strength of 45 Mpa at 28 days, except some of the samples which will be crushed at 56 days. Hopefully strength will be achieved at 56 days, as the fylash will contribute to the later strength gain.
The slab is post-tensioned. This localized spalling as visible in the enclosed pictures, we presume is due to high magnitude of poast tensioning load and also due to improper compaction with the vibrator during pouring as the slab is 2.0 metres deep and the slump of concrete is around 170mm.
Kindly evaluate the reasons for such failure of concrete.
We have observed spalling of concrete upon de-shuttering the soffit formwork after 25 days. The concrete slab is 2.0 meter thickness and was poured using 45 Mpa mix with 35% flyash to meet heat of hydration requirements as the thickness is 2.0 meters.
Test cylinder samples have achieved the required strength of 45 Mpa at 28 days, except some of the samples which will be crushed at 56 days. Hopefully strength will be achieved at 56 days, as the fylash will contribute to the later strength gain.
The slab is post-tensioned. This localized spalling as visible in the enclosed pictures, we presume is due to high magnitude of poast tensioning load and also due to improper compaction with the vibrator during pouring as the slab is 2.0 metres deep and the slump of concrete is around 170mm.
Kindly evaluate the reasons for such failure of concrete.