I have an existing concrete beam (interior) that is subject to constant high temperatures (around 142F, 62C). At the interface between the roof deck and the beam, concrete is spalling from the face of the beam. There is no visible stress cracks on the surface of the beam, the beam has not been subject to a fire, yet the spalling does not extend to the reinforcing steel within. The concrete used was normal density concrete, 5000#/si. Concrete cover to the steel was to be 2". The depth of the spalls are less than 2" in many areas, and where they extend deeper into the beam 2-2.5", no rebar has been exposed.
Any ideas as to the cause of the concrete spalling?