I am looking for a film or a chemical solution that will help to stop condensation from forming and gathering on our barcode reader/labels.

Thanks.

Alex Hussain
Instumentation Laboratory
Systems R & D
me_coop@ilrd.com
781 861 4448
 
Replies continue below

Recommended for you

If you want help, describe the problem with data.
Finding a solution without knowing the conditions and requirements is magic, not engineering.

<nbucska@pcperipherals.com>
 
What exactly is condensating?
Is it caused by local hot steaming, or general high humidity around?
Why would not you just blow on, probably with hot air?
 
Teflon or Parrafin coat the label so that water beads and runs off.
 