I am looking for conductive rubber sheet
approx 1mm thick with resistivity of 1K to 10K ohm/square, or similar.
I need strips for longitudinal sensing eg 150mm x 20mm
can anyone suggest a manufacturer??
 
Replies continue below

Recommended for you

dear sir
ref. your request we can do it.
 
wire iran co. thanks for reply. can you please send full info to michael.mestrovic@csiro.au
 
did you find your conductive rubber source?
If so, could you forward to me? I, too, am looking for something for a conductive, elastomeric seal or boot.

thanks
 
Try Tecknit at (908) 272 5500. They manufacture many different types of conductive rubber in sheet, rod, and other forms. they are located in Cranford, N.J.
 
Try Mearthane products in Cranton RI, USA.

They call themselves now MPC.
 