Hello All!
This is my first time here and I think this forum can be very informative!
I've been involved with control rod design criteria and one issue that has come up is the design lifetime. I have seen some plants have had problems (major & minor...) with unexpected events. How do you estimate/calculate how long a control rod (RCCAs, CEAs, etc) will last before failure? Is there an acceptable amount of damage before the control rod must be replaced (e.g., a 1/2 inch crack vs. 3 inch crack)?
Any info would be much appreciated!
This is my first time here and I think this forum can be very informative!
I've been involved with control rod design criteria and one issue that has come up is the design lifetime. I have seen some plants have had problems (major & minor...) with unexpected events. How do you estimate/calculate how long a control rod (RCCAs, CEAs, etc) will last before failure? Is there an acceptable amount of damage before the control rod must be replaced (e.g., a 1/2 inch crack vs. 3 inch crack)?
Any info would be much appreciated!