Starting on a new project. A small sugar cane processing plant in sunny Indonesia. We are scheduled to begin earthworks soon. Going to strip the vegetative layer (20 cm) and do a controlled fill with clay up to grade level for the main building. Total height of fill - 1 to 1.5m. I need help with specifying a QC procedure for this from the owner's side. Our spec is 95% MDD, 20cm lifts.
* Is it realistic to do sand cones on every lift? Several samples?
* I am planning to require a minimum size for the sand cone - 200mm cone with 4L jug.
* What is the proper equipment for compacting each lift? I have seen them simply rolling over the incoming fill with a dozer before. Dozer spreads and drives over, spreads and drives over.
* Is it realistic to do sand cones on every lift? Several samples?
* I am planning to require a minimum size for the sand cone - 200mm cone with 4L jug.
* What is the proper equipment for compacting each lift? I have seen them simply rolling over the incoming fill with a dozer before. Dozer spreads and drives over, spreads and drives over.