Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Corrosion Information

Status
Not open for further replies.

Chpal1984

Mechanical
Nov 19, 2014
31
Hi,

I was wondering if anyone on here can help me. I'm looking for corrosion data for Alloy 718, AM 350, Alloy 42 and 316 SS, when exposed to different fluids (e.g. Acetic acid, Acetyl Chloride, Acetone etc). I've tried my trusty NACE Corrosion Survey Database, but these metals aren't in it. Does anyone have any suggestions as to where I might find the data?

many thanks
 
Replies continue below

Recommended for you

They are different animals.
Alloy 42, if you are meaning Fe-42Ni, it is not even considered to be corrosion resistant. it will rust at humid environments even at room tempreature.
718 is a superally (high temp alloy)
Am350 is precipitate hardenable, general corrosion resistance is similar to 316
316 cannot be hardened by heat treatment.
 
Or the Compass corrosion guide.
Concentration, impurities, and temperature will be critical.
Though some of these, such as acetone will not effect any of these metals.

= = = = = = = = = = = = = = = = = = = =