Friends,
We want to develop a plan for corrosion monitoring of our subsea pipeline as well as onshore gas processing facility. I would like to know from someone who is involved in actual corrosion monitoring of such assets or systems how does one go about it? Presently we have provision for installing corrosion coupons at 2 locations. Besides coupons what other methods are in use? Our gas essentially is very sweet with no H2S only CO2. In short I would like to develop a comprehensive plan for corrosion monitoring for the subsea pipeline till the sales line on onshore plant.What would be the typical locations where it would be critical?
Thanks in advance pl
 
Replies continue below

Recommended for you

Here is the e-mail address of a colleague of mine who works in corrosion monitoring. I have forwarded him your enquiry. Hope they can help.

guy.tipton@capcissystems.com

regards