For small areas of cad plating that have worn, or been machined, off of steel and nickel-aluminum-bronze (e.g. bushings), what are folks seeing done to protect the surface without having to re-cad plate?
 
Replies continue below

Recommended for you

Could you tell us more about "brush cadmium plating"? Do you have material and application specification references by chance?

Thanks.
 
Actually, let me adjsut the question... a quick google brought up a lot of info... what spec seems to be the aero industry standard for this process?
 
Standards:

AMS 2451/4B --Plating, Brush, Cadmium Corrosion Protective, Low Hydrogen Embrittlement

AMS-QQ-P-416 --Plating, Cadmium (Electrodeposited)
 