Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations JStephen on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Could I make a carabiner's pin/rivet out of copper instead of steel? 8

Status
Not open for further replies.

panosjapan

Specifier/Regulator
Joined
Oct 22, 2014
Messages
18
Location
GR
Hi,
I am making a carabiner which won't be suitable for climbing, but designed mainly to carry keys.

In order to achieve a beautiful contrast, I want to make the pin/rivet of the carabiner out of copper.

Would that create a problem with the longevity of the carabiner? Is copper not strong enough to sustain the everyday use of a carabiner keychain?

Best,
Panos
 
What not PVD coat a steel pin with titanium nitride? It would be a beautiful gold color and would wear extremely well.

Maui

 
Maui said:
What not PVD coat a steel pin with titanium nitride? It would be a beautiful gold color and would wear extremely well.

Hi Maui and thanks for your reply. I didn't know about this process. I'll definitely look into it. Thanks!

Panos
 