Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations SSS148 on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Cozzone question

Status
Not open for further replies.

bf109g

Aerospace
Apr 8, 2008
177
I am working on determining maximum strength of a part we've been making for 30 years. All previous analyses have applied a load to the part to see if it can take it.

The cross section I have are two 1" high x .4" wide rectangles spaced at 4.5" with a .318" hole drilled parallel to the neutral axis and .375" from the bottom of the section. I am doing analysis similar to Bruhn page C3.8, Example 4 and can get a k1 of 1.5 for the upper section, but I get a k2 of less than 1 for the lower section. The upper section is critical under the worst load case - I don't think I have a strength problem with the part. I just want to analyze it correctly.

I've never come across a k value less than 1 before. I believe I can use Fb for the upper section and Ftu for the lower section. Does this sound reasonable?
 
Replies continue below

Recommended for you

i've never seen k < 1 ... i'm certain that by definition it can't be (so i suspect a calc problem) ... a rectangle section with a small piece removed should be darn close to 1.5.

 
That's what I'm thinking, too. Shouldn't be too far off 1.5, if at all.

Something's squirrelly here, I just haven't found it yet.
 