Chadarchie
Materials
- May 4, 2004
- 7
Has anyone ever dealt with cathodic protection in demineralized water with resistivity up to 6.25 million! Can anyone direct me to any reference regarding the corrosivity of this environment. From what I have been told the water is so starved of Fe that it will be aggressive in dissolving steel. I would think that there should be a different CP criteria (e.g. CP levels/current requirements etc.) to prevent this from happening.
The tank is internally coated which means I have to watch CP gradient so I don't blow the coating off.
Any input is appreciated. Thanks.
The tank is internally coated which means I have to watch CP gradient so I don't blow the coating off.
Any input is appreciated. Thanks.