We have applied on forging material (A 105N) the SSC test according to NACE TM177. After the termination time (720 hour) we have noticed the sample is broken (we completely observed the condition of test ex, sampling mechanic, applied force, test media,..) . Forge master has quite confidence to the material because Ceq is under 0.42 and also S Sulfur is under 0.03.
They are going to do metallographic study and get the result and specify the failure reasons.
But my question is: does any other method to assess and evaluation material respect to SSC compatibility? Or we shall do again SCC test in Lab.?
Is there any method to distinguish for this material is rejected without re- testing?
Please send me any information about this matter.
Thanks
They are going to do metallographic study and get the result and specify the failure reasons.
But my question is: does any other method to assess and evaluation material respect to SSC compatibility? Or we shall do again SCC test in Lab.?
Is there any method to distinguish for this material is rejected without re- testing?
Please send me any information about this matter.
Thanks