IgorPev
Mechanical
- Nov 11, 2012
- 17
Hi guys,
I would like to consult with the group regarding a failure I am experiencing in one of my injection molded parts.
The part is plastic shell enclosure made with injection molded PC/ABS (Chi Mei PC540), the screw socket is cracking in both of the bottom bosses. The cracks appear between 1-3 month after assembly, they may occur in storage or in the field.
I have tried to simulate the cracks myself without any successes, I have identified that there is a small gap (~0.2mm) between the two enclosures so some tensile stress may be applied.
The screw is a self-tapping type, the bosses does not show any singes of cracking, only the socket does.
Does anyone know how to test injection molded parts (not transparent) for stress / how to expedite cracking?
Does anyone experienced PC/ABS cracking this way before? (No oily / other solvents are present in the assembly line).
Thanks in advanced.
I would like to consult with the group regarding a failure I am experiencing in one of my injection molded parts.
The part is plastic shell enclosure made with injection molded PC/ABS (Chi Mei PC540), the screw socket is cracking in both of the bottom bosses. The cracks appear between 1-3 month after assembly, they may occur in storage or in the field.
I have tried to simulate the cracks myself without any successes, I have identified that there is a small gap (~0.2mm) between the two enclosures so some tensile stress may be applied.
The screw is a self-tapping type, the bosses does not show any singes of cracking, only the socket does.
Does anyone know how to test injection molded parts (not transparent) for stress / how to expedite cracking?
Does anyone experienced PC/ABS cracking this way before? (No oily / other solvents are present in the assembly line).
Thanks in advanced.