Hi,
I'm Xeros.

each material has specific creep temperature.
So, my client request the creep temperature for Cr-Mo steel and 25Cr-35Ni steel.

I could find web site for provide the creep temperature for material.

However, i think that data on web-site is not enough for reference to client.

Please give me the information about reference book title, code, standard or specification.

Best regards,
 
Replies continue below

Recommended for you

For Cr-Mo creep data, I would suggest the following publication (it is outdated but very comprehensive in terms of creep data) issued by the ASTM-ASME Joint Committee on Effect of High Temperature on the Properties of Metals or the web site below;

"Report on the Elevated-Temperature Properties of Chromium-Molybdenum Steels" Special Technical Publication No.151

For 25Cr-35Ni steels go here;

Note;
If you would like a printed version of a data sheet, please download and fill in the application form and send it by mail or email as a PDF file. Printed version of data sheet will be sent for free, only to those institutions whose applications have been approved by the Application Review Committee.


postal address: General Affairs S. of Meguro
National Institute for Materials Science
2-2-54 Nakameguro, Meguro-ku, Tokyo 153-0061, JAPAN
Fax. +81-3-3719-2177
email address:
the application form [PDF]
 
Please find below.

- API RP579, Table 4.1
- API STD 530, Annex E
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor