Please guide me to manufacture the vacuum insulated hose for liquid nitrogen
size - 1/2"
Pressure - 50 bar
temp - (-190 deg cel)
Should i take two sizes of SS bellow and weld it and create vacuum inside the cavity of the two hoses.
Or is there any simple method for this??
or simply 'Foamglas' insulated hose will work with same efficiency??
size - 1/2"
Pressure - 50 bar
temp - (-190 deg cel)
Should i take two sizes of SS bellow and weld it and create vacuum inside the cavity of the two hoses.
Or is there any simple method for this??
or simply 'Foamglas' insulated hose will work with same efficiency??