Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Cryogenic, Low Pressure RV

Status
Not open for further replies.

iainuts

Mechanical
Sep 24, 2003
552
Anyone know of a RV that can do this?

Inlet: 2"
Outlet: 3"'
Media: Helium gas
Temperature range: -440 F to 70 F
Set Pressure: 0.25 psig
Flow Required: 12,000 SCFH at -300 F
 
Replies continue below

Recommended for you

Just off the top of my head I would say talk to protectoseal. You really might want to go with a buckling pin if you are not setting it off all the time. Look at the PIN-TECH BUBBLE-TIGHT < 500 PPM, PRESSURE RELIEF VENT
Series No. 56000

My two cents

StoneCold
 
Thanks SC. I called them up, and although they don't have any cryogenic RV's, they seem interested in designing something.

Any other leads would be appreciated.
 
You might have trouble with the -440F. It seems more common for cryogenic valves to stop at around liquid nitrogen temps, around -325F. Other problem is the extremely low 0.25 psi set pressure, that's uncommon as well.


Not sure how low the Flowsafe valves go.
can make you a valve with materials accepted for cryo service, but they haven't tested them that way.

Best bet is probably an austenitic stainless body, like 316 SS.

Other materials to look for: Hastelloy, Inconel, Monel, aluminum (tho I haven't seen any Al valve), bronze/brass.

Only seal material I know of is teflon, but I've seen lots of different numbers on the lower temp limit.

Good luck.
 