HI Everybody here!
We are constructing a cryogenic LOX Tank. Min. temp -196 C, max is -20 . For now all pipe lines have been tested for pneumatic. Thte tank is ready for Hydrotest. Before hydrotest we are cleaning the tank with usin UV light Magnaflux 6000. For Cleaning actually must be used lint free cloth. But in our country market this material is not available and it takes time to be delivered.
But it is omportant to mention that when hydrotest finishes it will be cleaned again with chemical component and it will be pickled and passivated and this all will do another subcontractor.
My question is : do we have to wait lint free material or we can proceed with some clothes like Cheese Making Lint.
photos 1st : lint free cloth. 2nd Cheese Making Lint .3 spots in UV light
We are constructing a cryogenic LOX Tank. Min. temp -196 C, max is -20 . For now all pipe lines have been tested for pneumatic. Thte tank is ready for Hydrotest. Before hydrotest we are cleaning the tank with usin UV light Magnaflux 6000. For Cleaning actually must be used lint free cloth. But in our country market this material is not available and it takes time to be delivered.
But it is omportant to mention that when hydrotest finishes it will be cleaned again with chemical component and it will be pickled and passivated and this all will do another subcontractor.
My question is : do we have to wait lint free material or we can proceed with some clothes like Cheese Making Lint.
photos 1st : lint free cloth. 2nd Cheese Making Lint .3 spots in UV light