Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations KootK on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Current range value was specified in PQR when make tube to tubesheet qualification as per QW-288

Status
Not open for further replies.

Tony1t

Mechanical
Jun 18, 2012
22

Hi everyone,
A question was raised as current range value was specified in PQR when make tube to tubesheet qualification as per QW-288.

When I reviewed WPS for tube to tubesheet at shop found that a curent range value(235~300 A) was specified in WPS, alike a current range value (260~275 A) was also record in PQR which is used to supports the WPS. QW288.1 (m) said that a change of more than 10% in the current level from that qualified is need to requalified.

My question is that when make welding on product to use current value 300A that is exceeds the limit of 10%260A, is it acceptable to specified current range value in PQR &WPS like description above?
thanks in advance.
 