Hello.
I have problem with my design calculation for atmospheric tank. I cannot find the right thickness to use for the top cover flange.
Let me give some details:
Material shell= SS304L
Tank Outside diameter= 700mm
Tank shell length = 1300mm
Design pressure: Atm
Design temperature: 50 deg celcius
The tank is designed to have top cover so we plan to use customized OD800 X ID700 bolted flange and OD800 blind flange as top cover.
My colleague, from his previous company, used 10mm thick for the bolted flange but now we have to do some calculation to show that the thickness is enough
to hold 1 manhole on top of the cover.
Manhole dimension:
OD: 400mm
Length: 100mm
Material: SS304L
Will appreciate anybody's help. Thank you very much in advance!

Let me give some details:
Material shell= SS304L
Tank Outside diameter= 700mm
Tank shell length = 1300mm
Design pressure: Atm
Design temperature: 50 deg celcius
The tank is designed to have top cover so we plan to use customized OD800 X ID700 bolted flange and OD800 blind flange as top cover.
My colleague, from his previous company, used 10mm thick for the bolted flange but now we have to do some calculation to show that the thickness is enough
to hold 1 manhole on top of the cover.
Manhole dimension:
OD: 400mm
Length: 100mm
Material: SS304L
Will appreciate anybody's help. Thank you very much in advance!