GilPolymers
Materials
Hello,
I have long fibre reinforced composites samples with 10 x 50 x 2 (mm).
Composites have a thermoplastic matrix and glass fibres.
I'm trying to cut those composites in smaller samples of 5 x 5 x 2 without change their morphology.
I tried to cut those with a saw but the result was not so good, then I try to cut with a surgical knife but it was to hard, the 3rd attempt was using the same surgical knife but heated, it was nice but probably changes the polymer's morphology, finally I mad just some superficial cuts I put the composites in liquid nitrogen and I try to break them but the result was not the best.
someone has a better idea?!
Thanks in advance!
Pedro
I have long fibre reinforced composites samples with 10 x 50 x 2 (mm).
Composites have a thermoplastic matrix and glass fibres.
I'm trying to cut those composites in smaller samples of 5 x 5 x 2 without change their morphology.
I tried to cut those with a saw but the result was not so good, then I try to cut with a surgical knife but it was to hard, the 3rd attempt was using the same surgical knife but heated, it was nice but probably changes the polymer's morphology, finally I mad just some superficial cuts I put the composites in liquid nitrogen and I try to break them but the result was not the best.
someone has a better idea?!
Thanks in advance!
Pedro