HAS ANYONE CUT 1/2 OR 3/4" CORIAN? IF SO, I WOULD REALLY APPRECIATE IF YOU COULD SHARE CUT CONDITIONS. I CUT 1/2" FREQUENTLY, BUT CAN ONLY ACHIEVE 10 IPM; ANY FASTER AND THE EDGE TAPERS IN TOO MUCH AT THE BOTTOM OF IT. ANY ADVICE GIVEN IS GREATLY APPRECIATED.
I HAVE A MAZAK STX SUPER TURBO 1.5K. PRESENTLY I USE 800 WATTS WITH AIR.
THANKS
Gary L. Ellis Jr.
Quality Steel Fabrication
Sidney, OH
gellis@woh.rr.com
I HAVE A MAZAK STX SUPER TURBO 1.5K. PRESENTLY I USE 800 WATTS WITH AIR.
THANKS
Gary L. Ellis Jr.
Quality Steel Fabrication
Sidney, OH
gellis@woh.rr.com