I am not a machinist but in my work as a mechanical engineer I have to do some building which involves milling and turning and cutting.
Of all the materials I work with aluminium alloy sheets and plates ( eg AlMgSi 0.5 F22/6060 or HE30) gives most problems with poor finish and clogging of cutters, drills, hacksaw blades.
I am mainly using HSS toos without coolant.
Could someone give advice on speeds or cutter types for general purpose aluminium.
Thanks
Of all the materials I work with aluminium alloy sheets and plates ( eg AlMgSi 0.5 F22/6060 or HE30) gives most problems with poor finish and clogging of cutters, drills, hacksaw blades.
I am mainly using HSS toos without coolant.
Could someone give advice on speeds or cutter types for general purpose aluminium.
Thanks