Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Cylindrical roller bearing with increased speed. 1

Status
Not open for further replies.

dalcantara

Mechanical
Mar 23, 2004
3
Does anyone know about increasing the limiting speed of cylindrical roller bearings just by removing intercalated rollers from it? Is it a common thing?

I see that the basic dynamic load will decrease, but what happens with general tolerances? Why would it increase the limiting speed?

Thank you all,

Dalcantara
 
Replies continue below

Recommended for you

Removing rollers is no guarantee of a speed increase. Removing every other roller can cause out of balance problems which will distort the cage and quickly lead to a large failure.

Higher speeds are normally obtained through careful cage design and increased precision. Ultimately the idea is to get everything perfectly balanced at speed, ie higher ring concentricity through higher precision along with a strong more precise cage which will keep the rollers in check at higher speeds.

Sorry not to give an easy answer.

Regards

Neville
 
I've heard of it being done in special cases on some steel rolling mills.
No data of success.
 