Dear all
What tupe of evaporator should be used for caustic soda concentration up to 50%?
What construction materials should be used?
 
Solution
Material should be Nickel, based on my experience. Regarding operation, should be forced circulation due to the viscosity of caustic at high concentration.
Check physical properties of caustic solution. Pierre
Replies continue below

Recommended for you

There are a number of people out there with experience building these.
Steam heated.
There are only two material options, Ni200 or 26-1S (E-Brite) superferritic SS.
 
Material should be Nickel, based on my experience. Regarding operation, should be forced circulation due to the viscosity of caustic at high concentration.
Check physical properties of caustic solution. Pierre
 
Last edited:
Solution
Falling films could be considered as well or forced circulation is better?
 
Another resource:
You may want to contact them, both GEA and Alfa Laval
Pierre
 
Thank you so much, Pierre!
In my case, I need to project / specify a tubular unit.
 
I believe that Graham Mfg also makes these.
I have made a lot of E-Brite for this service, and have seen tubes with more than 40 years of service.
The issue with Ni200 is that it will erode from the excess salt in the solution.
 