Jul 19, 2024 #1 Akoll Mechanical Jun 20, 2023 8 0 0 IQ Dear All, which standard and level applicable for UT , for Forged Ring A105N OD 1580mm , ID 1275 mm and Th260 mm . Please advise which standard is applicable to do such test (UT)?
Dear All, which standard and level applicable for UT , for Forged Ring A105N OD 1580mm , ID 1275 mm and Th260 mm . Please advise which standard is applicable to do such test (UT)?
Jul 19, 2024 #2 Stick. Mechanical Feb 20, 2019 209 0 16 US I believe ASTM A388 would be a relevant standard for UT. Upvote 0 Downvote
Jul 19, 2024 Thread starter #3 Akoll Mechanical Jun 20, 2023 8 0 0 IQ what about this ASTMA578/A578MLEVELC ? Upvote 0 Downvote
Jul 19, 2024 #4 EdStainless Materials May 20, 2004 15,892 0 0 US Which is listed in the material specification? = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, consulting work welcomed Upvote 0 Downvote
Which is listed in the material specification? = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, consulting work welcomed
Jul 19, 2024 Thread starter #5 Akoll Mechanical Jun 20, 2023 8 0 0 IQ Not listed in the materials specification Upvote 0 Downvote
Jul 20, 2024 #6 EdStainless Materials May 20, 2004 15,892 0 0 US So there is no specification? Start by looking at ASTM casting specs for the same material and seeing what they refer to for NDT. = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, consulting work welcomed Upvote 0 Downvote
So there is no specification? Start by looking at ASTM casting specs for the same material and seeing what they refer to for NDT. = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, consulting work welcomed
Jul 20, 2024 #7 mfgenggear Aerospace Jan 23, 2008 2,699 0 36 US This https://www.astm.org/a0388_a0388m-19.html Upvote 0 Downvote