Zambo
Civil/Environmental
- Jun 5, 2003
- 697
We have a problem with the bridge deck waterproof membrane blistering during asphalting of the deck. The waterproof membrane is a mineral finished bitumen sheet membrane which is torched to the cut-back bitumen tack coat. The asphalt is 80mm thick and is laid in 2 layers, but blistering is happening during compaction of the first layer.