mrmalcolm
Marine/Ocean
- Jan 24, 2024
- 53
ISO 15614
8.4.4 Filler material, manufacturer/trade name, designation
Quote
For level 2: Filler materials cover other filler materials as long as, according to the designation in the appropriate international standard for the filler material, they have quivalent mechanical properties, same type of covering or flux core, same nominal chemical composition and the same or lower hydrogen content.
When impact testing is required by the application standard at temperatures less than −20 °C, for processes 111, 114, 12, 136 and 132 according to ISO 4063, the range of validity is restricted to the manufacturer trade name of the filler material used in the procedure test. In this case, it is also permissible to change the manufacturer of filler material to another with the same compulsory part of the designation provided one additional test piece is welded using the maximum heat input qualified and only weld metal impact test specimens shall be tested. This does not apply to solid wire and rods with the same designation and nominal chemical compositions.
Unquote
How to define and determine impact testing temperature required by the application standard?According to the impact test temperature of the base material or the impact test temperature of the welding consumable?
In some application standards, such as EN13445, assuming a service temperature of 0 ℃, the required base metal test temperature is -10 ℃. At this point, the manufacturer may choose welding consumables with an impact test temperature of -20 ℃. In this case, according to ISO 15614-1 8.4.4 level2 , what is the impact test temperature required by the application standard?
Feel free to give your comments.
8.4.4 Filler material, manufacturer/trade name, designation
Quote
For level 2: Filler materials cover other filler materials as long as, according to the designation in the appropriate international standard for the filler material, they have quivalent mechanical properties, same type of covering or flux core, same nominal chemical composition and the same or lower hydrogen content.
When impact testing is required by the application standard at temperatures less than −20 °C, for processes 111, 114, 12, 136 and 132 according to ISO 4063, the range of validity is restricted to the manufacturer trade name of the filler material used in the procedure test. In this case, it is also permissible to change the manufacturer of filler material to another with the same compulsory part of the designation provided one additional test piece is welded using the maximum heat input qualified and only weld metal impact test specimens shall be tested. This does not apply to solid wire and rods with the same designation and nominal chemical compositions.
Unquote
How to define and determine impact testing temperature required by the application standard?According to the impact test temperature of the base material or the impact test temperature of the welding consumable?
In some application standards, such as EN13445, assuming a service temperature of 0 ℃, the required base metal test temperature is -10 ℃. At this point, the manufacturer may choose welding consumables with an impact test temperature of -20 ℃. In this case, according to ISO 15614-1 8.4.4 level2 , what is the impact test temperature required by the application standard?
Feel free to give your comments.