Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations IRstuff on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Definition plastic strain (PE) abaqus 1

Status
Not open for further replies.

Crowner

Automotive
Nov 3, 2015
6
Hi everybody,
Ive been looking for the definition of the plastic strain (PE) output in Abaqus, how is this one computed? In the Users Manual are only informations about normal and logarithmic strain and i can't find anything in the Theory manual either.
Thanks a lot!
 
Replies continue below

Recommended for you

Hello,

Do you need Plastic strain formula? if so plastic strain = (Ln(1+ nominal strain))-(Ln(1+(true stress/elastic modulus)))

hope this helps
 
Hi, Thanks for your help, so abaqus simply calculates the nominal strain through the Deformation Tensor and substracts the elastic strain to get the plastic strain?
Regards
 
Not only Abaqus, this is the universal formula for plastic strain.
 