Hi All

I am completing pipe design calculations using UNS S31803 (65ksi yield) in an operating temperature range of -4F to 250F. I am trying to account for the shift in Young's modulus and yield strength at the elevated temperatures but need some advice.

ASME II Part D table Y-1 gives the temperature adjusted yield strength for a range of materials but unfortunately UNS S31803 is not on that list. Section 7-230 of ASME II states the guidelines for grade substitution (material composition needs to meet all the limits of the substituted material). There is a material that meets all the requirements except for N (table y-1's material specifies 1N and UNS S31803 has 0.08-0.2)

Can I use the adjusted yield for the material in Y-1 for UNS S31803?

Also is there any other standard that will give me the adjusted yield for UNS S31803 (I cannot find it in US DOT/FAA published "Metallic Materials Properties Development and Standardization(MMPDS)")

Thanks in advanced
 
Replies continue below

Recommended for you

Not sure what the issue is. S31803 (which is very similar to S32205) has the yield listed in table Y-1 as a function of temp.
Chart HA-5 applies to find related shift in Young's modulus as a function of temperature.

I'm looking at the 2019 edt., which is current.

Huub
- You never get what you expect, you only get what you inspect.
 
Hi X:83NL,

Thanks for the feedback. The problem is the Nitrogen content for S31803 does not match the Nitrogen content for S32205. Basically what I am asking is can I use S32205 inspite of this and if so why?

Kind regards
 
Im not sure if I understand your issue correctly. Table Y-1 lists the yield strength (and fig. HA-5 the E-modulus) as a function of T for S31803 (in the current edt of ASME ASME II), which to me seems to be what you're looking for. Then why look for a substitute material instead?