APDplastmold
Industrial
- May 16, 2013
- 7
We experience severe living hinge delamination problem. We suspect excessive 1.Frozen Skin formation and the consequential 2.high Shear rate/Shear stress during filling due to hesitation flow in the hinge caused by apparently improper gate location. The latter is too close to the hinge resulting in the following filling dynamics: while the gated side of the box fills relatively easily, the flow is slowly crossing through or even stopping in the hinge; the resultant, significant Frozen Skin restricts the flow channel. Due to the latter event and the sudden climb of injection flow rate through the hinge (after the completion of filling of the gated box half) the Shear rate rises remarkably causing high Shear stresses among the layers of laminar flow leading to delamination. We will run a precision Flow analysis to test this hypothesis. Please post another possibilities, help is appreciated in advance.
G. Markus
G. Markus