I am designing a flange to be integratated into a cast body so it need to be studded. I have had a look at ASME 16.5 and BS EN 1092-1 as the casting has to be design to machined to take a DN 50mm PN160 type 21 RF flange or a 2" ASME Class 600 Flange the casting is designed to take a maximum pressure of 160 Bar and will be cast from Cf8m or Duplex depending on the pressure and temperature of the application.

Most flanges i have designed for casting have a cast tube to the flange.

Do I design it to the required dimension given by ISO an ASME.

Or are there any further standard I need to look at espacailly with stud thread depth in to casting, stud type rolled or machined threads, and materal of studs.
 
Replies continue below

Recommended for you

Make sure that the "Area" of your cast-in flange is only dedicated to flange loads -- the body loading needs to be "held" by the calculated area without the volume of the flange.

Stud depth to be equal or a little deeper than a B16.5 studded flange. Rolled vs. cut threads are immaterial to ASME.

You have a great idea, just don't overcomplicate it. Also, make sure the casting house knows that the fully machined part will have to pass a hydrogen/helium 'bubble' test. ALL castings have internal shrink. It the caster lets the shrink get into the flange or stud areas, you have a "leaker" and it fails to meet Code.
 
Thanks for the reply do you know how suitalbl cf8m is for threaded stud, as it shaer strangth is around 205 Mpa

Thanks
 
CF8M = B8M
B8M is a standard stud material. Just have to design to its limitations. It is not a high-strength bolting material.
 
Sorry I meant C8FM for the threaded cast material,and stud bolts to be stainless steel grade a4-80.

thanks fro your help
 