Dear forum members,
I'd appreciate if anyone can shed some light on rubber modelling in abq CAE. I'm modelling an elastomer gasket using *Hyperelastic, Marlow. There are several sets of test data which I have tried to include in my inp deck, namely uniaxial, biaxial, planar and volumetric test data.
When running the inp deck, I received this error msg (which led to job termination)
***ERROR: ONLY ONE SET OF DEVIATORIC TEST DATA OPTION CAN BE USED WITH MARLOW
HYPERELASTICITY
***NOTE: DUE TO AN INPUT ERROR THE ANALYSIS PRE-PROCESSOR HAS BEEN UNABLE TO
INTERPRET SOME DATA. SUBSEQUENT ERRORS MAY BE CAUSED BY THIS OMISSION
Is this indicative of data overkill in the inp deck? Does this mean I have to remove some of the data?
Appreciate the help.
thanks,
jo
I'd appreciate if anyone can shed some light on rubber modelling in abq CAE. I'm modelling an elastomer gasket using *Hyperelastic, Marlow. There are several sets of test data which I have tried to include in my inp deck, namely uniaxial, biaxial, planar and volumetric test data.
When running the inp deck, I received this error msg (which led to job termination)
***ERROR: ONLY ONE SET OF DEVIATORIC TEST DATA OPTION CAN BE USED WITH MARLOW
HYPERELASTICITY
***NOTE: DUE TO AN INPUT ERROR THE ANALYSIS PRE-PROCESSOR HAS BEEN UNABLE TO
INTERPRET SOME DATA. SUBSEQUENT ERRORS MAY BE CAUSED BY THIS OMISSION
Is this indicative of data overkill in the inp deck? Does this mean I have to remove some of the data?