Petroleum
May 4, 2012
4
Can we substitue AFLAS O-Ring with BUNA O-Ring?
 
Replies continue below

Recommended for you

I'll say "probably not, but maybe." Depends entirely on the fluid, pressure, and temperature.

Good on ya,

Goober Dave

Haven't see the forum policies? Do so now: Forum Policies
 
Ok, thank you very much for your help. What is the usage for BUNA O-Ring?
 
"What is the usage for BUNA O-Ring?"

Cheap stuff that you don't mind having leak past the o-ring.

More seriously, google "Parker O-ring Handbook", download it, read it, and become an o-ring expert very quickly.
 
The industry trend in my area of interest (upstream oil and gas) is to specify the Aflas in moderately sour service and / or in amine service. Buna does not last as long or perform as well in those services, apparently.
 
There is a world of difference in the materials, Aflas being a Fluoropolymer and Buna-N being a Nitrile Rubber. Though both have their limitations the Aflas covers more ground, though at a higher cost.
A key point is if you are able, is to check it out in the fluid you are going to exposed to. A simple immersion test will tell you a lot as most charts are for pure materials.


 