Does anybody have a cut sheet for stainless steel 304, butt welded reducing tees? I need the radius for the transition from the run to the branch in a 3" x 1½" SCH 10S tee (MSS SP-43).
If I can show that there is actually a radius, then I can reduce the pipe entrance flow loss in my pressure drop calculation.

Clyde
 
Replies continue below

Recommended for you

I don't think the standards call out an internal (wetted surface) radius. That leaves you a couple of options: One - go to your warehouse and measure a few samples and specify the same manufacturer for your project. Two - talk to a manufacturer's engineer for guidance. One which has some online info is Weldbend at
jt
 
jte (Mechanical)

Thank you for the detail technical link
 
Thanks for the ideas. I had considered measuring a tee out of our store room.

If I can use a r/d of at least 0.02 for a 3"x1½" reducing tee instead of assuming a square edge, my RV inlet piping pressure drop calc will drop from 4.6% of set pressure to 2.7% (which satisfies the <3% guideline). When I get this radius measured, I will post up the results.

Looks like I will be leaning on this forum more in the future.